隐藏筛选条件产品名称 | 产品分类 | 导热率 W/mk | 体积电阻 @23℃ Ohm-cm | 粘度 cps @23℃ | 触变指数 | 玻璃化温度 | 储能模量 psi@23℃ | 固化条件 | (邵氏)硬度 | 操作 |
---|---|---|---|---|---|---|---|---|---|---|
H20E-SLR-MX | 导电胶 | 1.21 | 0.004 | 4341cps @50rpm | 4.1 | 78 | 1041110 | 140℃/35sec 120℃/15min 100℃/2hrs 80℃/4hrs | - | |
P1011 | 导电胶 | 2.74 | 0.0005 | 8000-12000cps @20rpm | 1.9 | - | upon | pre bake: 30min@80℃, cure 1hr@150℃,post cure 90min@285℃ | - | |
H20E-FC | 导电胶 | 2.63 | 0.0004 | 2361cps @100rpm | 4.62 | 85 | 927509 | 140℃/35sec 120℃/15min 80℃/45min | - | |
H20E-SLR | 导电胶 | 1.21 | 0.004 | 4424 | - | 81 | 1041110 | 140℃/35sec 120℃/15min 100℃/2hr 80℃/4hr | - | |
H31D-LV | 导电胶 | 0.89 | 0.008 | 10000-15000@20rpm | 1.6 | ≥110 | 310264 | 150/1hr | 85 | |
H31LV | 导电胶 | 0.55 | 0.008 | 2000-3500 | 1,8 | ≥110 | 257143 | 150/1hr | 85 | |
H22 | 导电胶 | 0.94 | 0.005 | 12000-2000cps @20rpm | 2.36 | ≥100 | 540120 | 150℃/5min 120℃/10min 100℃/20min
| 80 | |
EV2118-2 | 导电胶 | 4.03 | 0.0005 | 2849 | - | 40 | 685789 | 150℃/10min 120℃/20min 100℃/1hr
| - | |
H21D | 导电胶 | 1 | 0.0009 | 14000-20400cps @20rpm | 2.6 | ≥100 | 802491 | 150℃/5min 120℃/15min 80℃/90min | 60 | |
EE149-6 | 导电胶 | 0.98 | 0.0005 | 2000-4000@100rpm | 4.7 | ≥130 | 546505 | B-Stage: 70°C/10min Cure: 180°C/1hr | 74 | |
EJ2189 | 导电胶 | 1.38 | 0.0005 | 55000-90000cps @1rpm | 5.2 | ≥30 | 275557 | 150/℃/15min 100℃/1hr 80℃/3hr 23℃/3day | - | |
H24 | 导电胶 | 0.67 | 0.02 | 15000-23000@10rpm | 1.86 | ≥100 | 484807 | 150℃/5min 120℃/10min 100℃/20min 80℃/45min | 76 | |
H20E-LV | 导电胶 | 2.5 | 0.0004 | 1800-2800cps @100rpm | 3.43 | ≥80 | 640479 | 175°C/45 Sec - 150°C/5 min - 120°C/15min - 80°C/3 hr | - | |
E4110 | 导电胶 | 1.37 | 0.0005 | 800-1600cps @100rpm | - | ≥40 | 518756 | 150℃/15min 100℃/60min 80℃/3hr 60℃/6hr 23℃/3day | - | |
T6067 | 导热胶 | 0.45 | - | 300000-400000@1rpm | N/A | 90 | 641860 | 150℃/1hr; 120℃/2hr | - |